EFOX BPIC S75

EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene within the temperature range of 95 to 125 °C. During polymerization, the temperature is gradually increased. EFOX BPIC S75 can be used as an initiator for the solution copolymerization of acrylates and methacrylates within the temperature range of 100 to 170 °C, including for the production of coatings. EFOX BPIC S75 can also be used as an initiator for the bulk and suspension copolymerization of acrylates and methacrylates.

EFOX BPIC S75
Chemical Name
Tert-Bütil Peroksi İzopropil Karbonat 75%
Yoğunluk (@20°C) Viskozite (@20°C) Görünüm Renk
0,900 ± 0,005 gr/cm3 2,3 mPa.s Sıvı Renksiz
Aktif Oksijen İçeriği Peroksit İçeriği (BPIC%) Hidroperoksit (TBHP) Toplam Klor İçeriği
6,72 - 6,90 % 74,0 - 76,0 % Max. 0,10 % Max. 150 ppm
SADT CAS No EINECS/ELINCS No UN No
70°C 2372-21-6 219-143-7 3103
PROPERTIES

EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene within the temperature range of 95 to 125 °C. During polymerization, the temperature is gradually increased. EFOX BPIC S75 can be used as an initiator for the solution copolymerization of acrylates and methacrylates within the temperature range of 100 to 170 °C, including for the production of coatings. EFOX BPIC S75 can also be used as an initiator for the bulk and suspension copolymerization of acrylates and methacrylates.